Super-Duplex Seawater Coolers: Material, Welding and Testing

At a glance. Offshore platforms and coastal plants cool lube oil, seal gas, glycol and compressed gas with seawater. Seawater pits and crevice-corrodes 316L, and copper alloys suffer in polluted or fast-flowing water. Super duplex stainless steel (UNS S32750, often called 2507) resists chloride attack at a fraction of the cost of titanium or nickel alloys, but only when it is welded and tested correctly.
Why super duplex
Pitting resistance. Super duplex has a pitting resistance equivalent number (PREN) above 40, against about 25 for 316L.
Strength. Its yield strength is roughly twice that of 316L, so tubes, shells and tubesheets can be thinner.
Stress-corrosion cracking. The two-phase structure resists chloride stress-corrosion cracking far better than austenitic stainless steels.
Cost. It costs much less than titanium and most nickel alloys, and it welds in a normal workshop.
Titanium remains the choice for the warmest and most strongly chlorinated seawater. The right alloy depends on temperature, chlorination and flow, and should be agreed at enquiry.
Where the welds go wrong
Super duplex is roughly half ferrite and half austenite. Too much heat input, slow cooling or the wrong filler upsets that balance or forms brittle intermetallic phases such as sigma. The weld then corrodes and cracks long before the base metal. Good practice includes:
Qualified procedures with controlled heat input and interpass temperature.
Over-alloyed filler metal and suitable shielding and backing gas.
Ferrite measurement on procedure qualification welds and on production welds.
Corrosion and intermetallic tests on the procedures, for example to ASTM G48 and ASTM A923.
What to ask for in the dossier
Material certificates for tubes, plate and forgings, and positive material identification (PMI) of every alloy part.
Weld procedure and welder qualifications, with ferrite, hardness and corrosion test results.
Radiography or other volumetric testing to the design code.
Hydrotest records, with water quality controlled to avoid chloride deposits.
Sour-service compliance (NACE MR0175 / ISO 15156) where the process side needs it.
Choosing the construction
Fixed tubesheet coolers cost least when the shell side stays clean.
U-tube and floating head bundles can be pulled for cleaning and handle thermal expansion.
Hairpin units give long thermal length in a short footprint, with true counter-current flow.
Long tubes, up to about 6 m, often avoid a second shell. Replacement bundles can be built to the original drawing at turnarounds.
Where Tech Inc. equipment fits
Tech Inc. builds the super-duplex seawater cooler range, high-pressure hairpin heat exchangers and special-alloy replacement tube bundles, and fits coolers into its lube-oil consoles and seal-gas conditioning skids. Our welders are qualified on duplex, super duplex and nickel alloys.
Related reading
Sources
ASTM A923, Detecting Detrimental Intermetallic Phase in Duplex Austenitic/Ferritic Stainless Steels – ASTM International
ASTM G48, Pitting and Crevice Corrosion Resistance of Stainless Steels and Related Alloys by Use of Ferric Chloride Solution – ASTM International
NORSOK M-001:2025, Materials selection – Standards Norway
TEMA Standards – Tubular Exchanger Manufacturers Association
This guide is general information. Material selection and testing follow the design code, the project specification and the operator's standards.