Hollow Fibre Membrane Making Equipment Compared: Spinning Lines, Spinnerets and Module Building


Bottom line: start fibre development on the lab hollow fibre casting machine and interchangeable spinnerets. Move to the pilot spinning line for longer runs, and to the commercial line for 2 to 8 spinnerets. Build modules with the potting centrifuge, resin dosing machine and guillotine, then check them on the integrity tester.
Spinning, coating and post-treatment
Machine | Scale | Speed | Dope and spinneret | Other data |
|---|---|---|---|---|
laboratory | adjustable take-up speed | dope and bore metering pumps; interchangeable spinneret tips | coagulation bath with temperature control; adjustable air gap; PVDF, PES, PSf, PAN | |
laboratory | take-up up to about 30 m/min | single or multi-hole spinneret | bath about 1 m; draw ratio set by godet speeds | |
pilot | up to about 50 m/min | heated dope tank 5 to 50 L; single, multi or dual-layer spinnerets | air gap 0 to 30 cm | |
production | 5 to 60 m/min | 2 to 8 spinnerets; dope up to 120 °C (248 °F) | SS304 or SS316 wetted parts | |
1, 4 or 8 braids | 2 to 30 m/min | dope up to 90 °C (194 °F) | braid about 1.5 to 2.5 mm | |
1 or 4 fibres | 0.5 to 20 m/min | – | fibre OD 0.3 to 3 mm; oven up to 150 °C (302 °F) | |
all lines | – | annulus OD 0.5 to 3 mm; needle OD 0.2 to 1.5 mm | SS316 or SS304; heating jacket option | |
about 50, 200 or 500 L tanks | – | – | water ambient to 80 °C (176 °F); SS304 or SS316 |
Module building and testing
Machine | Function | Size range | Key data |
|---|---|---|---|
centrifugal potting of fibre bundles | modules to 0.3, 0.7 or 2 m | variable speed up to several hundred rpm; chamber ambient to 60 °C (140 °F); PU and epoxy | |
doses and mixes two-component resin | heated tanks 5 to 30 L | ratio 100:10 to 100:100; shot about 5 g to 2 kg; PU, epoxy, silicone | |
cuts potted hollow fibre modules | module diameter up to about 110 mm | hardened stainless blade; manual or pneumatic; guard and two-hand control | |
pressure decay, bubble point and diffusion tests | modules up to about 2 m | test pressure up to 3 bar (44 psi) | |
bench-scale membrane bioreactor for module trials | – | submerged module; aeration for biology and air scour; suction pump |
How to choose
Fibre development needs fine control of dope, bore fluid, air gap and take-up speed, so start in the laboratory before committing to a line.
Spinneret geometry sets fibre size and wall thickness: choose the orifice count and sizes for your target fibre.
Reinforced or composite fibres need a braid or coating line rather than a plain spinning line.
Plan potting, cutting and integrity testing with the spinning line so module lengths and diameters match.
All models: hollow fibre membrane making.
Before you order
Send us your samples, operating conditions and the standard you work to, and we will confirm the model. Equipment carries our standard warranty and installation, training and service terms: see Service and Support and our Terms of Sale. Send an enquiry or email mail@techincresearch.com.
Data are typical and taken from each product page and datasheet; final design is to the client specification and the order acknowledgement. Check the product page or ask us before you order.