top of page

Formation Factor, Resistivity Index and Archie's a, m and n

Writer: Tech Inc
Tech Inc
5 hours ago
1 min read

At a glance. Formation factor is the resistivity of a brine-saturated core divided by the brine resistivity. Resistivity index is the core's resistivity at partial saturation divided by its fully saturated value. Plotting them gives Archie's cementation exponent m and saturation exponent n. The Tech Inc. Formation Resistivity and Capillary Pressure Tester measures both.

Archie's equations

  • Formation factor: F = Ro ÷ Rw = a ÷ φ^m

  • Resistivity index: I = Rt ÷ Ro = Sw^−n

Measuring well

  • Use four-electrode measurement to remove contact resistance.

  • Measure at a fixed frequency (about 1 kHz) to avoid electrode polarisation.

  • Desaturate on a porous plate so the brine stays evenly distributed.

  • Keep temperature steady: brine resistivity changes about 2% per °C.

Typical values

Rock

m

n

Clean sandstone

about 1.8 to 2.0

about 2

Vuggy carbonate

can exceed 2.5

can exceed 2.5

Shaly sand

needs clay correction

needs clay correction

Frequently asked questions

Why not use default values? A change of m from 2.0 to 2.3 can shift water saturation by many saturation units in low-porosity rock.

Is a confining stress needed? It improves realism, especially for unconsolidated or fractured rock.